The activation energy of the reduction process was found to be 47.21±2.83 kJ/mol. Therefore, the decomposition of zinc ferrite by iron powder could be carried out at 1 atm with low pyrometallurgical temperature (600°C) and equipped with hydrometallurgical process to obtain high zinc yield.